ASTM, 2013, 4p. ASTM A744 / A744M. Standard Specification for Castings, Iron-Chromium-Nickel, Corrosion Resistant, for Severe Service
Brief Summary
This specification covers standard requirements for iron-chromium-nickel alloy, stainless steel castings intended for particularly severe corrosive applications. Alloys shall be melted by the electric furnace process with or without refining such as argon-oxygen-decarburization. Castings shall be heat treated and shall conform to the required heat treatment conditions. The materials shall conform with the prescribed chemical requirements for carbon, manganese, silicon, phosphorus, sulfur, chromium, nickel, molybdenum, columbium, copper, selenium, tungsten, vanadium, iron, and nitrogen.
Scope
This specification covers iron-chromium-nickel alloy, stainless steel castings intended for particularly severe corrosive applications.
This specification requires postweld heat-treatment of all weld repairs affecting surfaces intended to be wetted by the corrosive medium. For applications for which postweld heat-treatment is not considered mandatory for retention of acceptable corrosion resistance, refer to Specification A743/A743M.
Note For general corrosion-resistant alloy castings, reference should be made to Specification A743/A743M. For general heat-resistant alloy castings, reference should be made to Specification A297/A297M. For nickel-base alloy castings, refer to Specification A494/A494M.